Europe style for 1.52 Mm Pvb - Solar Backsheet – Xiaoshi
Europe style for 1.52 Mm Pvb - Solar Backsheet – Xiaoshi Detail:
TPT (solar backsheet) symplectite coatings contain highly dispersed nano titanium silicide and high thermal conductivity materials, which greatly improve the High-FluoroCocrystal solar cell backsheet performance. The high scratching resistance gets rid of these shortcomings of traditional coating, such as the surface of anti-scratch performance is poor, during the coating operation it is easy to get scratches or peel off, thus affecting the backsheet anti-ageing properties, etc. The High Reflectivity improves the light’s second reflection, enhances module output power, and increases the competitiveness of client module.High Heat Dissipation improves power generation efficiency of the backsheet by accelerating heat dissipation.
Product description and advantages
High Fluorine created the interconnected penetrate technology of high fluorine symplectite, with organic integration of the multi-fluoride raw material——Enhance the anti-ageing capability, improves weather resistance. Ripple-free high-precision coating technology makes coating of the surface smooth, and the uniform consistent——Enhance the density of the surface coating, improves electrical insulation properties. Nano-titanium silicide plasma processing techniques to enhance durable surface energy——Upgrades package compatibility, improves adhesion of EVA and silicone binding agent
1. High Weather Resistance
Through the accelerated ageing test of double-85 for 1000 hours, there will be non-delamination, non-cracking, non-foaming, as well as non-yellowing, no embrittlement after ageing by artificial ultraviolet radiation exposure (QUVB) test for 3000 hours.
2. High Security
Security grade has passed the flame-retardant UL94-V2 flame-retardant grade. The UL flame spread index is less than 100, which effectively guarantees the module security features.
3. High insulation
TUV Rheinland of PD>=1000VDC (based on HFF-300), which can avoid electrical arcing module.
4. High Water Vapor Resistance
By infrared water vapor permeability tester, the water vapor permeability rates≤1.0g/m2.d.
5. High Adhesion
After the nano-plasma treatment, the surface energy of high fluoride levels can last 45mN/m or more within six months.
6. High-end Match
Suitable for large-scale photovoltaic power plants with the crystalline silicon cells module package.
7. High Compatibility
Good compatibility comes from the bonding with the other packaging materials of module.
8. High Efficiency
For its double-sided adhesion, there’s no need to distinguish the backsheet’s positive and negative when components packaging, which brings convenience for technicians.
9. High Flexibility
The adhesive data of the bone package for the module and EVA could be adjusted as per the clients’ requirements.
Technical Data
Item | Unit | Standard | Value | |
Backsheet Thickness |
Nominal Value | mm | GB/T 31034-2014 | 0.28 |
Nominal Tolerance | N/A | N/A | ±5% | |
Tensile Strength (MD/TD) | Mpa | GB/T 31034-2014 | 146/138 | |
Elongation at break(MD/TD) | % | GB/T 31034-2014 | 110/130 | |
Thermal Shrinkage(MD/TD) | % | GB/T 31034-2014 | 0.68/0 | |
Coating Adhesion | Grade | GB/T 31034-2014 | 0 | |
Backsheet/EVA Peeling strength | N/cm | GB/T 31034-2014 | 80 | |
Backsheet/Silicone Peeling strength | N/cm | GB/T 31034-2014 | 12 | |
Breakdown Voltage | KV | GB/T 31034-2014 | 21.6 | |
Volume Resistivity | Ω . M | GB/T 31034-2014 | ≥1.0*1013 | |
Maximum Systen Voltage | V | GB/T 31034-2014 | 1125 | |
Moisture Vapor Transmission Rage | g/m2 *24 H | GB/T 21529-2008 | 1.07 | |
Damp-heat Testing (85℃,85%RH, 3000H) | N/A | GB/T 31034-2014 | No delamination, blister or crack, not significantly sticky on the surface and adhesive layer | |
UV Treatment(60kWh/M2) | N/A | GB/T 16422.2-1999 | △b≤3/ No delamination, blister or crack, not significantly sticky on the surface and adhesive layer, △b≤3 | |
Boiling water Treatment(24H) |
Apparent | N/A | GB/T 31034-2014 | No delamination, blister,discoloration or fold, not significantly sticky on the surface and adhesive layer |
Coating Adhesion | Grade | GB/T 31034-2014 | 0 | |
Hot and Cold Cycle processing ( -40 to 85℃, 6H/Cycle, 200 cycles) |
N/A | GB/T 31034-2014 | No delamination, blister,discoloration, crack or fold, not significantly sticky on the surface and adhesive layer | |
Damp-Frozen processing (-40 to 85℃,85%RH, 24H/Cycle, 10cycles) |
N/A | GB/T 31034-2014 | No delamination, blister,discoloration or fold, not significantly sticky on the surface and adhesive layer | |
Acid Resistance | N/A | GB/T 31034-2014 | No delamination, blister or discoloration | |
Alkali Resistance | N/A | GB/T 31034-2014 | No delamination, blister or discoloration | |
Salt spray Resistance | N/A | GB/T 2423.17-2008 | No delamination, blister, cracking or powdering, no significant discoloration | |
Solvent Resistance | Times | GB/T 31034-2014 | ≥1000 |
Product detail pictures:
Related Product Guide:
We insist on offering premium quality manufacturing with superior business concept, honest product sales as well as finest and fast assistance. it will bring you not only the good quality product or service and huge profit, but the most significant is to occupy the endless market for Europe style for 1.52 Mm Pvb - Solar Backsheet – Xiaoshi , The product will supply to all over the world, such as: Libya, Liberia, America, As the world economic integration bringing challenges and opportunities to the xxx industry, our company , by carrying on our teamwork, quality first, innovation and mutual benefit, are confident enough to supply our clients sincerely with qualified merchandise, competitive price and great service, and to build a brighter future under the spirit of higher, faster, stronger with our friends together by carrying on our discipline.
By Lindsay from Cologne - 2018.03.03 13:09
The factory technical staff not only have high level of technology, their English level is also very good, this is a great help to technology communication.
By Lilith from Bulgaria - 2018.06.30 17:29